Rubber Bearing Technical index |
Natural Rubber(-40ºC-60ºC) | Neoprene Rubber(-25ºC-60ºC) | |
Hardness(lRHD) |
60±5 | 60±5 | |
Tensile Strength(MPa) | ≥18 |
≥17 | |
Elongation at Break(%) |
≥450 | ≥400 | |
Brittleness Temperature(ºC) |
≤-50 | ≤-40 | |
Compression Set(70ºCx24h)(%) |
≤30 | ≤15 | |
Ozone Aging Resistance(20% strain,40ºC x 96h) |
25 pphm | 100 pphm | |
No Cracks | No Cracks | ||
Hot Air Aging | Test Condition(ºC x h) |
70x168 | 100x70 |
Max Change in Tensile Strength(%) |
-15 | -15 | |
Max Change in Elongation at Break(%) | -20 | -40 | |
Max Change in Hardness(lRHD) |
-5,+10 | 0,+10 | |
Bond Strength Between Elastomer and Steel Plate(KN/m) |
>10 | >10 | |
Bond Strength Between Elastomer and PTFE(KN/m) |
>7 | >7 |